Short answer: we roll pure nickel strip in Ni200, Ni201, N4 and N6, thickness 0.05 - 3.5 mm, width 2 - 300 mm, slit with a burr-free edge, in coils.
| Grade | Ni % | ρ20 (μΩ·m) | Typical use |
|---|---|---|---|
| Ni200 | ≥99.6 | 0.096 | General battery tabs, busbars |
| Ni201 | ≥99.0 (low C) | 0.096 | Where welded joints see higher temperature |
| N4 | ≥99.9 | 0.096 | High-purity requirement |
| N6 | ≥99.5 | 0.096 | General purpose |
| Item | Range | Tolerance |
|---|---|---|
| Thickness | 0.05 - 3.5 mm 0.002" - 0.138" | ±0.02 mm (<0.2 mm) ±0.03 mm (0.2-1.0 mm) ±0.05 mm (>1.0 mm) |
| Within-coil thickness spread | - | ≤5 % of nominal (tighter on request) |
| Width | 2 - 300 mm 0.079" - 11.8" | ±0.15 mm (<20 mm) ±0.25 mm (20-100 mm) ±0.40 mm (>100 mm) |
| Edge | - | Slit, burr height ≤0.02 mm, deburred |
| Camber (bow) | - | ≤2 mm per metre |
| Condition | - | Annealed soft (typical for tabs) |
| Coil | - | ID 300 mm, 20-80 kg, interleaved |
| Thickness × width | Weight per metre | Metres per kg |
|---|---|---|
| 0.10 × 5 mm | 4.45 g/m | 225 m |
| 0.15 × 8 mm | 10.7 g/m | 94 m |
| 0.20 × 10 mm | 17.8 g/m | 56 m |
| 0.30 × 20 mm | 53.4 g/m | 19 m |
Basis: density 8.9 g/cm³. Weight per metre = thickness × width × 8.9 ÷ 1000 (mm, kg/m).
Send grade, form, size with tolerance and quantity — we reply within one working day (GMT+8).
WhatsApp +86 136 6174 5686 Enquiry formShanghai Xinxiang Alloy Materials Co., Ltd. was founded in 2014 and is a source manufacturer of electric heating alloys and nickel-based precision alloys. Production base in Taixing, Jiangsu, approximately 20,000 m², 48+ pieces of melting, forging, rolling, drawing, heat-treatment and testing equipment, 200+ staff, annual capacity about 7,500 tonnes.
Contact: Tel +86 136 6174 5686 / +86 21 6911 6339 | Email shryhjcl@126.com
Grade cross-references are commercial equivalents, not a guarantee of interchangeability. Final acceptance is subject to the composition sheet agreed at order.