FeCrAl · Ni-Cr · Pure Nickel · Precision Alloys  |  +86 136 6174 5686EN|中文|RU|ES
Xinxiang AlloyXinxiang AlloySHANGHAI XINXIANG

Grade reference: 15 electric heating and resistance alloys

Composition windows, resistivity, maximum service temperature and typical applications. All values are typical; confirm against the mill certificate for your batch.

FeCrAl heating alloys

GradeCr %Al %ρ20 μΩ·mMax temp. °CTypical use
0Cr25Al520.0–23.04.5–6.51.401,300General high-temperature furnaces, continuous operation
0Cr21Al6Nb20.0–23.05.0–7.01.42–1.451,350Better high-temperature strength, long spans
0Cr27Al7Mo226.0–28.06.0–7.51.531,400Ultra-high temperature, large element spans
1Cr13Al412.0–15.03.5–4.51.251,000Low-temperature, cost-sensitive applications
0Cr23Al522.0–24.04.5–5.51.351,250Intermediate between 1Cr13Al4 and 0Cr25Al5

Ni-Cr and Ni-Cr-Fe

GradeNi %Cr %ρ20 μΩ·mMax temp. °CTypical use
Cr20Ni8075.0–78.020.0–23.01.091,200Frequent cycling, vibration, welding
Cr15Ni6055.0–58.015.0–18.01.121,100Medium temperature, cost-performance balance
Cr30Ni7068.0–72.028.0–31.01.181,250High nickel, corrosion resistance
Cr20Ni3534.0–37.018.0–21.01.041,100Ni-Cr-Fe, good oxidation resistance

Pure nickel and copper-nickel

GradeNi %ρ20 μΩ·mMax temp. °CTypical use
Ni200≥99.60.096600Low-voltage heating, battery tabs, corrosion resistance
N4 / N6≥99.50.096600Same as Ni200, Chinese designations
6J40 (Constantan)39.0–41.00.48400Precision resistors, shunts, thermocouples
Manganin2.0–3.0 Mn, 11.0–13.0 Mn0.44–0.48300Standard resistors, low thermal EMF

Precision resistance alloys

GradeCompositionρ20 μΩ·mTCR ppm/°CTypical use
6J12Cu-Mn0.43–0.47±20Precision resistors
6J20Ni-Cr1.08–1.12±10Precision resistors, strain gauges
6J40Cu-Ni (Constantan)0.48±20Shunts, thermocouple negative leg

Selection notes

Pick by three numbers: service temperature, atmosphere and cycling frequency.

Need a recommendation?

Send the furnace type, service temperature, atmosphere and element span. We will reply with a grade and the surface-load figure to work to.