FeCrAl · Ni-Cr · Pure Nickel · Precision Alloys  |  +86 136 6174 5686EN|中文|RU|ES
Xinxiang AlloyXinxiang AlloySHANGHAI XINXIANG

How to choose a heating alloy grade: three numbers

Temperature, atmosphere, cycling. Get these three right and the grade choice is usually obvious.

There are dozens of grades and the datasheets all look similar. In practice, three numbers decide most of it.

Number one: element temperature

Not furnace temperature. The element runs 50–150 °C hotter than the furnace, so the grade must be rated above the element temperature, not the furnace temperature.

Element temperatureSuitable grades
below 800 °C1Cr13Al4, Cr15Ni60
900–1,000 °CCr15Ni60, 0Cr25Al5
1,000–1,100 °C0Cr25Al5, 0Cr21Al6Nb
1,100–1,200 °C0Cr21Al6Nb
1,200–1,300 °C0Cr27Al7Mo2
above 1,300 °Cspecial alloys or non-metallic elements

Number two: atmosphere

AtmosphereNote
Air / oxidisingnormal use for both families
Nitrogenfine, but watch the oxygen partial pressure
Hydrogenreducing — attacks the oxide film, avoid FeCrAl
Vacuummetal evaporates; heating alloys are generally unsuitable
Carburisingcarbon pick-up embrittles the element
Sulphur-bearingsevere corrosion

When the atmosphere is aggressive, Ni-Cr is the safer default.

Number three: cycling frequency

PatternRelative life
Continuous, 2 stops a year100%
2 stops a week70–80%
1 stop a day45–55%
3+ stops a day25–35%

Frequent cycling favours Ni-Cr because of its toughness.

Putting them together

Example 1 — 1,000 °C, air, continuous. 0Cr25Al5. Cheapest grade that meets the requirement. Example 2 — 1,000 °C, air, 3 stops a day. Cr20Ni80. Costs more, but survives the cycling. Example 3 — 1,200 °C, air, continuous. 0Cr21Al6Nb or 0Cr27Al7Mo2. Example 4 — 900 °C, hydrogen, continuous. Not a good fit for heating alloys. If it must be used, Cr20Ni80 at a reduced surface load.

The one mistake to avoid

Choosing the highest grade "to be safe". Higher grades are more brittle, harder to form, and more expensive. They do not automatically last longer — they last longer only if the operating conditions actually require them.

Related

Grade reference · Request a quote